Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00550 cm/cm
0.00550 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 137 MPa
19900 psi
ASTM D638
Elongation at Break 2.50 %
2.50 %
ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Unnotched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Descriptive Properties Value Comments
Color Black