A. Schulman POLYBATCH™ Bright While LL80250 Concentrate Based In LLDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Bright While LL80250 Concentrate Based In LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® LL80250 is a bright white masterbatch containing 50% titanium dioxide based in LLDPE. This product has been formulate to provide a brighter, cooler, more fresh appearance over standard white color concentrates. POLYBATCH® LL80250 also offers optimal dispersion and excellent letdown mixing. POLYBATCH® LL80250 is typically recommended for use at 2% addition levels in blow molding applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 50 %
50 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789
Pellet Count 32
pellets/gram