Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Time 86400 sec
0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 123 MPa
17800 psi
Type I, 5 mm/min; ASTM D638
123 MPa
17800 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
Type I, 5 mm/min; ASTM D638
2.4 %
2.4 %
ASTM D638
Flexural Strength 188 MPa
27300 psi
1.3 mm/min, 50 mm span; ASTM D790
188 MPa
27300 psi
ASTM D790
Flexural Modulus 9.37 GPa
1360 ksi
1.3 mm/min, 50 mm span; ASTM D790
9.37 GPa
1360 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.79 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved