Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.374 J/cm @Thickness 3.17 mm |
0.700 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 0.374 J/cm @Thickness 3.17 mm |
0.700 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 0.374 J/cm @Thickness 3.17 mm |
0.700 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 0.374 - 16.4 J/cm | 0.700 - 30.7 ft-lb/in | Average value: 5.72 J/cm Grade Count:9 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Unnotched | 0.374 - 7.47 J/cm | 0.700 - 14.0 ft-lb/in | Average value: 3.28 J/cm Grade Count:13 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.374 J/cm @Temperature -40.0 °C |
0.700 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |