Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6BK Nylon 6 Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 228 °C | 420 - 442 °F | ASTM D789 |
Niche Polymer PA6GF33BK Nylon 6, 33% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF43BK Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | Molding |
PolyOne Edgetek® AS-20GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 216 °C | 420 °F | |
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Melt Temperature | 216 °C | 420 °F | |
Teknor Apex Chemlon® 217 GI Nylon 6, 17% Glass Fiber Reinforced Features: High Impact, 17% Glass Reinforced; Highly toughened compound designed to improve practical toughness and ductility Processing Method: Injection Molding Forms: Pellets Additive: Impact Mod.. |
|||
Melt Temperature | 216 °C | 420 °F | |
Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Inj.. |
|||
Melt Temperature | 216 °C | 420 °F | |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 - 274 °C | 420 - 525 °F | Average value: 257 °C Grade Count:22 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |