Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00550 cm/cm | 0.00550 in/in | ASTM D955 |
Niche Polymer PA6GF13BK Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00550 cm/cm | 0.00550 in/in | ASTM D955 |
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00550 cm/cm | 0.00550 in/in | ASTM D955 |
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00550 cm/cm | 0.00550 in/in | Average value: 0.00550 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |