Niche Polymer PA6GF13BK Nylon 6, 13% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PA6GF13BK Nylon 6, 13% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00550 cm/cm
0.00550 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.45 MPa
500 psi
ASTM D638
Elongation at Break 5.00 %
5.00 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Unnotched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 193 °C
380 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Descriptive Properties Value Comments
Color Black