Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded , Polyurethane, TP
Manufacturer A. Schulman, Inc.
Trade Name POLYPUR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYPUR™ CB 1110 Thermoplastic Polyurethane Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
0.0090 - 0.014 cm/cm

@Thickness 3.20 mm,
Time 259000 sec
0.0090 - 0.014 in/in

@Thickness 0.126 in,
Time 72.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
15 sec delay; ASTM D2240
Tensile Strength, Ultimate 37.0 MPa
5370 psi
2 in/min, at max load; ASTM D638
44.0 MPa
6380 psi
20 in/min, at max load; ASTM D412
Elongation at Break 380 %
380 %
20 in/min; ASTM D412
Flexural Modulus 0.835 GPa
121 ksi
ASTM D790
Tear Strength 226 kN/m
1290 pli
2 in/min; ASTM D624
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C

@Temperature -30.0 - 30.0 °C
83.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
Copyright © lookpolymers.com All Rights Reserved