Solvay Chemicals Trisodium hexafluoroaluminate

Category Ceramic , Halide
Manufacturer Solvay Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Chemicals Trisodium hexafluoroaluminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Solvay
Physical Properties Metric English Comments
Molecular Weight 210 g/mol
210 g/mol
Thermal Properties Metric English Comments
Melting Point 1009 - 1012 °C
1848 - 1854 °F
Descriptive Properties Value Comments
Appearance Powder, Crystalline
Color Slightly colored
Composition >95%
Trisodium hexafluoroaluminate