Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 138 MPa | 20000 psi | |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 13 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 138 MPa | 20000 psi | 2mm/min; ASTM D790 |
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
IDI Composites A-203 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 AF10 Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionInformation provided by.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 T/AL20 HS 10% Aramid Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Aramid Fiber, 10% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated, Heat Stabilized, Low Friction .. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES Luriblend® TPX-PA6/6-01072 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerAdditive: Molybdenum Disulfide LubricantFeatures: Lubricated, Low Friction and Good Wear ResistanceInformation provided b.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 HS MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedTPCI# 9094101Information provided by TP Composites, Inc. |
|||
Flexural Strength | 138 MPa | 20000 psi | |
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Adell AH-38 Nylon 66, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
Applied Composites 8092 Polyester SMC Industry Application: ConstructionProduct Application: Building ProductsDistinct Features: Pigmentable, High Molding Efficiency, Low Thermal ExpansionInformation provided by Applied Composites Corpo.. |
|||
Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
A. Schulman ComAlloy Voloy® 685 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.48% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Strength | >= 138 MPa | >= 20000 psi | |
Bulk Molding Compounds BMC 845 30% Glass Filled Vinyl Ester BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at .. |