Axiall 21540 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 21540 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
delayed; ASTM D-2240
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D-638
Elongation at Yield 255.9 %
255.9 %
Air Aging: 7 days @ 121°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 32 %
32 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
50% RH; ASTM D-257
Dielectric Constant 2.56

@Frequency 1e+6 Hz
2.56

@Frequency 1e+6 Hz
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F