Material Notes:
Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide. Glass-Bonded Mica is the only inorganic material to bridge the performance materials gap between organic plastics and ceramics.This unique high performance technical ceramic is a union of finely powered electrical quality glass and precisely defined and classified mica. The union of mica and glass takes place under simultaneous pressure and heat, transforming the materials into a new composition that inherits all the insulating advantages of both constituents.These materials are easily machined, mold like plastic, and have a wide range of operating temperatures. They find applications in the aircraft, laser, communications, aerospace, cryogenic, electronic, radiation, semiconductor, computer, automotive, and power distribution industries.Typical data below provided by Mykroy/Mycalex Ceramics.
Physical Properties Metric English Comments
Density 2.50 g/cc
0.0903 lb/in³
Moisture Absorption at Equilibrium 0.00 %
0.00 %
Nil
Mechanical Properties Metric English Comments
Hardness, Rockwell A 46
46
Hardness, Rockwell H 90
90
Tensile Strength, Ultimate 41.4 MPa
6000 psi
Modulus of Elasticity 75.8 GPa
11000 ksi
Flexural Strength 89.6 MPa
13000 psi
Compressive Strength 310 MPa
45000 psi
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 350 °C
6.11 µin/in-°F

@Temperature 662 °F
12.5 µm/m-°C

@Temperature 25.0 °C
6.94 µin/in-°F

@Temperature 77.0 °F
Specific Heat Capacity 0.5021 J/g-°C
0.1200 BTU/lb-°F
Thermal Conductivity 0.870 W/m-K
6.04 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 400 °C
752 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Surface Resistivity per Square 1.00e+9 ohm
1.00e+9 ohm
Dielectric Constant 6.7

@Frequency 1e+6 Hz
6.7

@Frequency 1e+6 Hz
Dielectric Strength 28.7 kV/mm
730 kV/in
Dissipation Factor 0.0018

@Frequency 1e+6 Hz
0.0018

@Frequency 1e+6 Hz
Dielectric Loss Index 0.012
0.012
1 MHz
Arc Resistance 245 sec
245 sec
Descriptive Properties Value Comments
Color Dark Grey