Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
X-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
X-Direction; ASTM D3386-94 |
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance Features and Benefits:Significantly improved oxidation resistance compared to typical thermoset microwave materialsDesigned for performance sensitive, high volume applicationsLow loss - Excellent el.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 500 °C |
6.11 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
Austenitic |
Goodfellow Nickel 55/Titanium 45 Shape Memory Alloy Shape memory alloy is a description applied to that group of metallic materials which show the ability to return to the previously defined shape or size when subjected to the correct thermal procedu.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 425 °C |
6.11 µin/in-°F @Temperature 68.0 - 797 °F |
|
Crucible Steel CPM® REX® 66 (HS) High Speed Steel CPM Rex 66 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed with a high vanadium content for excellent abrasion resistance, simila.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 315 °C |
6.11 µin/in-°F @Temperature 32.0 - 599 °F |
|
Crucible Steel Maxel® 2000 Stainless Steel Maxel 2000 is a free-machining stainless holder block steel which is based on the nominal analysis of Type 414L rather than Type 420. It is supplied pre-hardened to about HRC 37. Due to its unique c.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 95.0 °C |
6.11 µin/in-°F @Temperature 68.0 - 203 °F |
|
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 900 °C |
6.11 µin/in-°F @Temperature 69.8 - 1650 °F |
Mean |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.11 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature <=538 °C |
6.11 µin/in-°F @Temperature <=1000 °F |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 93.0 °C |
6.11 µin/in-°F @Temperature 69.8 - 199 °F |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition TH 1050 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.11 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter Chrome Core® 12-FM Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |