Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 89.6 MPa | 13000 psi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers PC-1029 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings 211 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
I. Stern N1921 General Purpose Crystal Polystyrene Features:Excellent ProcessabilityEasy FlowApplicationsDisposable PackagingHousewaresCosmetics PackagingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. In.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES Plaslube® J-80/20/TF/15 NAT Acetal (POM) Copolymer |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive) Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall 9275J Amber 05 Rigid PVC, Molding, Amber 05 Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved.Information pro.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall 9275J Clear 40 Rigid PVC, Molding, Clear 40 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall CL-6380, CL-6380J Rigid PVC, Molding Georgia Gulf CL-6380 & CL-6380J are clear fittings compounds with cell class 12454(Type 1, Grade 1). These compounds are ideally suited for swimming pools, spas, and numerous applications where vis.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS Information provided by Asahi Thermofil |