Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name Supreme
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and high peel strength, plus the convenience of a fast cure at low temperatures if desired. This new one component adhesive system is formulated to cure by exposure to a wide range of elevated temperatures.
Physical Properties Metric English Comments
Viscosity 120000 - 135000 cP

@Temperature 23.0 °C
120000 - 135000 cP

@Temperature 73.4 °F
Storage Temperature 23.9 °C
75.0 °F
6 months
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Processing Properties Metric English Comments
Cure Time 4.98 - 9.60 min

@Temperature 149 °C
0.0830 - 0.160 hour

@Temperature 300 °F
19.8 - 30.0 min

@Temperature 121 °C
0.330 - 0.500 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Color Yellow to Brown