Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature 350 °C |
6.11 µin/in-°F @Temperature 662 °F |
|
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
Y-Direction; ASTM D3386-94 |
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
X-Direction; ASTM D3386-94 |
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 500 °C |
6.11 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-7-120NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance moldi.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 100 - 200 °C |
6.11 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature >=100 °C |
6.11 µin/in-°F @Temperature >=212 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 204 °C |
6.11 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.0 - 204 °C |
6.11 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 300 °C |
6.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-KF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 95.0 °C |
6.11 µin/in-°F @Temperature 68.0 - 203 °F |
|
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 600.0 °C |
6.10 µin/in-°F @Temperature 1112 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 25.0 - 300 °C |
6.11 µin/in-°F @Temperature 77.0 - 572 °F |
|
Carpenter Chrome Core® 12 Alloy Data provided by Carpenter Technology Corporation.Chrome Core® alloys are a family of controlled chemistry, ferritic 8 and 12% chromium-iron alloys which are candidates for use in magnetic componen.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |