Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.870 W/m-K | 6.04 BTU-in/hr-ft²-°F | |
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
Thermal Conductivity | 0.870 W/m-K | 6.04 BTU-in/hr-ft²-°F | ASTM D177 |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.870 W/m-K @Temperature 100 °C |
6.04 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Thermal Conductivity | 0.870 W/m-K | 6.04 BTU-in/hr-ft²-°F | ASTM D5470 |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |