Hong Kun Group AO 626 Antioxidant

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group AO 626 Antioxidant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: Bis(2,4-di-tert-butylphenyl)pentaerythritol diphosphiteCAS No. 26741-53-7All information provided by Hongkun Group
Physical Properties Metric English Comments
Volatiles <= 1.0 %
<= 1.0 %
Thermal Properties Metric English Comments
Melting Point >= 170 °C
>= 338 °F
Chemical Properties Metric English Comments
Acid Value <= 1.0
<= 1.0
mg KOH/g
Descriptive Properties Value Comments
2,4-Di tert butylphenol (%) <= 1
Appearance white powder