Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubriplate CP-8A Petroleum-Based Gear, Bearing, & Recirculating Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate CP-8A Petroleum-Based Gear, Bearing, & Recirculating Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This non-EP (Extreme Pressure) oil is manufactured with acidless tallow as required to meet AGMA specification 8A Comp. It is recommended for use in cone drives and double-enveloping worm gear drives. CP-8A is available in Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 95
95
Viscosity Index
1000
1000
ISO Grade
Saybolt Viscosity at 100°F 4950 SUS
4950 SUS
Saybolt Viscosity at 210°F 230 SUS
230 SUS
Kinematic Viscosity at 40°C (104°F) 950 cSt
950 cSt
Kinematic Viscosity at 100°C (212°F) 47 cSt
47 cSt
Thermal Properties Metric English Comments
Pour Point 1.67 °C
35.0 °F
Flammability Test 600
600
[°F] Fire Point
Flash Point 288 °C
550 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 250
Users viewing this material also viewed the following: