Material Notes:
Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded or injection molded. Features:Permanently static dissipativeHumidity insensitiveUltra-Clean: low off-gassing, low ionic contaminationColorableDurable: Can be used repeatedly.No carbon/particulate fillersApplications:Cleanroom suppliesSemiconductor handlingElectronic component handlingDisk PackagingProperties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material three to four hours at 70°C (160°F) in a dehumidifying hopper dryer. Data provided by Noveon, Inc.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Tensile Modulus 0.862 GPa
125 ksi
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790-90
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256-93a
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+10 ohm-cm
6.00e+10 ohm-cm
50% RH; ASTM D257
Surface Resistance 8.00e+8 ohm
8.00e+8 ohm
ESD S11.11; 50 % R.H.
Surface Resistivity per Square 8.00e+9 ohm
8.00e+9 ohm
50% RH; ASTM D257
Static Decay 0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (+5000 V to 50 V)
0.010 sec
0.010 sec
FTMS-101C; 12% R.H., (-5000 V to -50 V)
0.50 sec
0.50 sec
Charged Plate Monitor; 50% R.H.
Tribocharge 10 V
10 V
Nitrile Glove - BFG Test Method
Processing Properties Metric English Comments
Drying Temperature 70.0 °C
158 °F
Dry Time 3 - 4 hour
3 - 4 hour
Descriptive Properties Value Comments
Color Light Blue