I. Stern WC-102 General Purpose Crystal Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer I. Stern & Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern WC-102 General Purpose Crystal Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityComplies with FDA Title 21 CFR 177.1640ApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 1.75 g/10 min
1.75 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.6 MPa
6900 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.8 °C
199 °F
ASTM D648
Vicat Softening Point 107 °C
225 °F
ASTM D1525
Flammability, UL94 HB
HB