Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 8.00e+9 ohm | 8.00e+9 ohm | 50% RH; ASTM D257 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Surface Resistivity per Square | 8.00e+9 ohm | 8.00e+9 ohm | 50% RH; ASTM D257 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |