Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.00e+10 ohm-cm | 6.00e+10 ohm-cm | 50% RH; ASTM D257 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Volume Resistivity | 6.00e+10 ohm-cm @Temperature 120 °C |
6.00e+10 ohm-cm @Temperature 248 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |