Polymer Property : Tensile Modulus = 0.862 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.862 GPa
125 ksi
1% Secant; 50mm/min; ASTM D638
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Tensile Modulus 0.862 GPa
125 ksi
ASTM D638
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene
Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES..
Tensile Modulus 0.862 GPa
125 ksi
ASTM D638
Westlake Plastics Kynar® 2850 PVDF Copolymer
Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab..