Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mechanical properties, chemical resistance and processability for very demanding applications.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ISO 868
Hardness, Shore D 52
52
ISO 868
Tensile Strength, Yield 35.06 MPa
5085 psi
ISO 527-2/5A/500
Elongation at Break 600 %
600 %
ISO 527-2/5A/500
50% Modulus 0.0100 GPa
1.45 ksi
ISO 527-2/5A/500
100% Modulus 0.01100 GPa
1.595 ksi
ISO 527-2/5A/500
300% Modulus 0.0190 GPa
2.76 ksi
ISO 527-2/5A/500
Tear Strength 150 kN/m
855 pli
Unnicked; ISO 34-1B
Abrasion 25
25
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 124 °C
255 °F
ISO 306
Processing Properties Metric English Comments
Zone 1 200 - 210 °C
392 - 410 °F
Zone 2 205 - 215 °C
401 - 419 °F
Zone 3 215 - 225 °C
419 - 437 °F
Zone 4 220 - 230 °C
428 - 446 °F
Adapter Temperature 200 - 230 °C
392 - 446 °F
5
Die Temperature 225 - 235 °C
437 - 455 °F
6
225 - 235 °C
437 - 455 °F
TIP, 7
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F