Polymer Property : Zone 2 = 419 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 195 - 215 °C
383 - 419 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec..
Zone 2 185 - 215 °C
365 - 419 °F
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr..
Zone 2 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane
Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica..
Zone 2 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar..
Zone 2 205 - 215 °C
401 - 419 °F
Injection
Lubrizol Estane® GP 55 DB Thermoplastic Polyurethane
Type: Estane® GP 55DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Features: Translucent spherical pellets.Uses: Injection molding partsAvailable in EuropeInformation Provided by..
Zone 2 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 52DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 2 205 - 215 °C
401 - 419 °F
Injection
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..
Zone 2 190 - 215 °C
374 - 419 °F
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances ..
Zone 2 205 - 215 °C
401 - 419 °F
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..