Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0100 GPa | 1.45 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
50% Modulus | 0.0100 GPa | 1.45 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
50% Modulus | 0.0100 GPa | 1.45 ksi | DIN 53504 |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.0100 GPa | 1.45 ksi | ISO 37 |
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in .. |
|||
50% Modulus | 0.0100 GPa | 1.45 ksi | ISO 37 |
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |