Polymer Property : 300% Modulus = 0.0190 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0190 GPa
2.76 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec..
300% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-7180 Polycaprolactone Based TPU
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 4 PHR Di-Cup 40C
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical)
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.0190 GPa
2.75 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0190 GPa
2.76 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-2195 Polycaprolactone Based TPU
Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0190 GPa
2.76 ksi
Dow Pellethane® 2354-45D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-45D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane..