Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Selar® PA 2072 Nylon Barrier Resin

Category Polymer , Film , Thermoplastic , Nylon , Nylon, Barrier Film Copolymer
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Selar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Selar® PA 2072 Nylon Barrier Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Selar® PA 2072 is an amorphous nylon (polyamide) resin which is specially designed for blending with ethylene vinyl alcohol (EVOH) copolymers. Selar® PA 2072 can be tumble-blended with most grades of EVOH to form blends which combine the excellent barrier properties of EVOH with the deep-draw thermoforming properties, processing flexibility and moisture-insensitivity of Selar® PA. In addition, Selar® PA 2072 provides better adhesion in blends with EVOH than other grades of amorphous nylon, and this may allow converters to use less expensive adhesives.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 70.0 MPa
10200 psi
ASTM D882
Film Elongation at Break, MD 20 %
20 %
Orientation not specified; ASTM D882
Flexural Modulus 2.80 GPa
406 ksi
at 50% RH; ASTM D790
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 125 °C
257 °F
ASTM D3418
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D1003