Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01100 GPa | 1.595 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
100% Modulus | 0.01100 GPa | 1.595 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11H98 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining a unique set of properties such as mec.. |
|||
100% Modulus | 0.01100 GPa | 1.595 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |