Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.dynamic stressBearings, sleeves, control disks, gear wheels, cams.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Stress 200 MPa
29000 psi
Elongation at Yield 1.8 %
1.8 %
2.3 %
2.3 %
flexural
Modulus of Elasticity 24.0 GPa
3480 ksi
Flexural Strength 290 MPa
42100 psi
Flexural Modulus 20.0 GPa
2900 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
180 °C
356 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
Electrical Properties Metric English Comments
Surface Resistance <= 100 ohm
<= 100 ohm
Insulation Resistance <= 100 ohm
<= 100 ohm
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
mass temp
Nozzle Temperature 265 - 275 °C
509 - 527 °F
Zone 1 285 - 295 °C
545 - 563 °F
Zone 2 270 - 280 °C
518 - 536 °F
Zone 3 265 - 275 °C
509 - 527 °F
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
120 °C

@Time 7200 - 18000 sec
248 °F

@Time 2.00 - 5.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)