Material Notes:
Densified laminated woodInformation provided by elisto
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Flexural Strength 140 MPa

@Temperature 23.0 °C
20300 psi

@Temperature 73.4 °F
Flexural Modulus 15.0 GPa
2180 ksi
Compressive Strength 270 MPa

@Temperature 23.0 °C
39200 psi

@Temperature 73.4 °F
Descriptive Properties Value Comments
Application Temperature (°C) 110