Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon Fiber Reinforced
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved friction and wear behaviour. Emergency running property.High dimensionally stable precision parts.Body and duty parts in office equipment, gear wheels, grippers.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ISO 1183
Water Absorption <= 0.20 %
<= 0.20 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 110 MPa
16000 psi
Elongation at Yield 2.0 %
2.0 %
2.5 %
2.5 %
flexural
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 165 MPa
23900 psi
Flexural Modulus 8.50 GPa
1230 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
flatwise; ISO 179 1fU
2.10 J/cm²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179 1eA
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179 eA
Coefficient of Friction, Dynamic 0.19
0.19
Coefficient of Friction, Static 0.16
0.16
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C
17.2 µin/in-°F
DIN 53752
Thermal Conductivity 0.470 W/m-K
3.26 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 130 °C
266 °F
150 °C
302 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
Vicat Softening Point 160 °C
320 °F
DIN ISO 306
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance <= 1e+05
<= 1e+05
Insulation Resistance <= 1.00e+6 ohm
<= 1.00e+6 ohm
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F
mass temp
Nozzle Temperature 290 - 310 °C
554 - 590 °F
Zone 1 280 - 300 °C
536 - 572 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 300 - 320 °C
572 - 608 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color dust grey