Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 10.0 - 1000 GPa | 1450 - 145000 ksi | |
NanoAmor 50% Regular Single Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an.. |
|||
Modulus of Elasticity | 10.0 - 16.0 GPa | 1450 - 2320 ksi | Injection; ISO 527 |
Raschig Group 5553 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Modulus of Elasticity | 10.0 - 14.0 GPa | 1450 - 2030 ksi | Injection; ISO 527 |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1105-7907 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 50-1375 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/BK Polyamide 66, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS-B Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and .. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/BK Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | |
Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Modulus of Elasticity | 10.0 GPa @Thickness >=1.50 mm |
1450 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart.. |
|||
Modulus of Elasticity | 10.0 GPa @Thickness >=1.50 mm |
1450 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Modulus of Elasticity | 10.0 GPa @Thickness >=1.50 mm |
1450 ksi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry) Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr.. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | Transverse |
Goodfellow Carbon/Epoxy Composite Rod Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Modulus of Elasticity | 10.0 - 17.2 GPa | 1450 - 2500 ksi | Average value: 12.8 GPa Grade Count:52 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Modulus of Elasticity | 10.0 GPa | 1450 ksi | ISO 527-2 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |