Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ G-4285-405 Black PVC Compound Application: A UV resistant, PVC based compound, suitable for extrusion applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | B |
Reltek BONDiT™ B-4682 Adhesive and Sealant Key PropertiesExcellent adhesion to low surface energy plastics without primeror surface preparation. ApplicationsHigh flexibility, 300% elongation, emphasizing high tack for un-abraded substrates a.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | B |
Reltek BONDiT™ B-451 Adhesive and Sealant Key PropertiesFlexible system for potting, painting, primer and protective coating applications. Excellent adhesion to low surface energy plastics. High chemical resistance. Ease of use.Applications.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | B |
Reltek BONDiT™ B-45EC Adhesive and Sealant Key PropertiesElectrically conductive without metal. High conductivity in three axes. Light weight, high chemical resistance. ApplicationsConductive adhesive designed with state-of -the-art extrinsi.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ISO 1183 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 844-10/176-CRB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
Sylvin Technologies 8950-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer Notes: 105°C Jacket; RoHS Compliant Uses Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Colorite Polymers 6283MG General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | DAM; ASTM D792 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Specific Gravity | 1.42 - 1.48 g/cc | 1.42 - 1.48 g/cc | ASTM D 792 |
Karina E 840-10/176-CRA White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |