Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Gear parts for automotive appliances, control disks, cams, sliding elements.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 240 MPa
34800 psi
Elongation at Yield 1.5 %
1.5 %
1.8 %
1.8 %
flexural
Modulus of Elasticity 22.0 GPa
3190 ksi
Flexural Strength 345 MPa
50000 psi
Flexural Modulus 19.0 GPa
2760 ksi
Charpy Impact Unnotched 4.90 J/cm²
23.3 ft-lb/in²
edgewise; ISO 179 1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C
11.1 µin/in-°F
DIN 53752
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 150 °C
302 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) >= 290 °C
>= 554 °F
Electrical Properties Metric English Comments
Surface Resistance <= 1000 ohm
<= 1000 ohm
Insulation Resistance <= 10000 ohm
<= 10000 ohm
Processing Properties Metric English Comments
Processing Temperature 310 °C
590 °F
mass temp
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Zone 1 285 - 315 °C
545 - 599 °F
Zone 2 305 - 315 °C
581 - 599 °F
Zone 3 305 - 315 °C
581 - 599 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color natural color (black)