Polymer Property : Maximum Service Temperature, Air = 320 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
short period, no load (dry sample)
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH
Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i..
Maximum Service Temperature, Air 160 °C
320 °F
P & P Technology EC-J Silver Aluminum Loaded Silicone
P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties..
Maximum Service Temperature, Air 160 °C
320 °F
NextGen Adhesives G907-28 Potting Adhesive
Description: NGAC G907-28 is a medium viscosity adhesive system formulated with a spherical glass filler to provide light weight and low shrinkage performance.Advantages and Applications: The NGAC G..
Maximum Service Temperature, Air 160 °C
320 °F
< 50 h; IEC 216/T1
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
Maximum Service Temperature, Air 160 °C
320 °F
< 50 h; IEC 60216/T1
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Maximum Service Temperature, Air 160 °C
320 °F
Cured
Resin Technology Group EN 239-2 Cationic UV Cure Epoxy Adhesive
EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resist..
Maximum Service Temperature, Air 160 °C
320 °F
Resin Technology Group EN 239-2 Millennium™ UV Curable Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Maximum Service Temperature, Air 160 °C
320 °F
Intermittent
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products  (discontinued **)
ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and ..
Maximum Service Temperature, Air 160 °C
320 °F
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Maximum Service Temperature, Air 160 °C
320 °F
< 50 hours; IEC 60216-P1
Hexion Bakelite™ PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, switch..
Maximum Service Temperature, Air 160 °C
320 °F
< 50 hours; IEC 60216-P1
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, ..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec..
Maximum Service Temperature, Air 160 °C
320 °F
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS/BK Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Improved friction and wear behaviour. Emergency running propert..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1-0889-4 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1-7984 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Maximum Service Temperature, Air 160 °C
320 °F
Intermittent
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry
Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH
Maximum Service Temperature, Air 160 - 220 °C
320 - 428 °F
Sichuan Deyang Haton® hs12370 Polyphenylene Sulfide Coating
Suspension; anti-corrosionInformation provided by Sichuan Deyang Chemical Co., LTD
Maximum Service Temperature, Air 160 °C
320 °F
Dry Service
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m..
Maximum Service Temperature, Air 160 °C
320 °F
short term; EMS
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I
Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610..
Maximum Service Temperature, Air 160 °C
320 °F
short term; EMS
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30
Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat..
Maximum Service Temperature, Air 160 °C
320 °F
short term; EMS
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15
Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop..
Maximum Service Temperature, Air 160 °C
320 °F
short term; EMS
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15
Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit..
Maximum Service Temperature, Air 160 °C
320 °F
ChevronTexaco Wheel End Grease
FeaturesChevron Wheel End Grease is a high performance grease specifically engineered for trailer wheel-ends operating in most conditions.It is formulated with ISOSYN™ base stocks, a unique polyure..
Maximum Service Temperature, Air 160 °C
320 °F
5000 h; VDE 0304/P2-1, IEC 216
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass
Characteristics: 30% glass fibre filled
Maximum Service Temperature, Air 160 °C
320 °F
short period, no load
Omnia Plastica Omniamid PA6 G G - Dry
Cast nylon 6. The method of production of this polyamide (i.e. the polymerisation of the caprolactam directly in the mould) allows the production of stock shapes in larger than normal dimensions, su..
Maximum Service Temperature, Air 160 °C
320 °F
short term
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..