Polymer Property : Nozzle Temperature = 626 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Average value: 325 °C Grade Count:3
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7342 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7950 Polyamide 46, with aramid reinforcement and PTFE, toughness-modified, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-8250 Polyamide 46, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-0664 Polyphthalamide, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-0778/BK Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-7314 Polyphthalamide, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-7970 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Nozzle Temperature 310 - 330 °C
590 - 626 °F
Injection Molding
LG Chemical LUCON PN9008 PPS+MF+GF
Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212..
Nozzle Temperature 310 - 330 °C
590 - 626 °F
Injection Molding
LG Chemical LUCON PN9009 PPS+MF
Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2..
Nozzle Temperature 290 - 330 °C
554 - 626 °F
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 290 - 330 °C
554 - 626 °F
Injection Molding
LG Chemical LUPOY GP2102 PC+GF10%
Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 290 - 330 °C
554 - 626 °F
LG Chemical LUPOY GP-2400 General Purpose Modified PC, 40% Glass Fiber Reinforced, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Average value: 325 °C Grade Count:4
Overview of materials for Polyphthalamide (PPA), Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a..
Nozzle Temperature 320 - 330 °C
608 - 626 °F
Average value: 325 °C Grade Count:7
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..