Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Gear parts for automotive appliances, control disks, cams, sliding elements.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Stress 225 MPa
32600 psi
Elongation at Yield 1.4 %
1.4 %
1.8 %
1.8 %
flexural
Modulus of Elasticity 23.0 GPa
3340 ksi
Flexural Strength 325 MPa
47100 psi
Flexural Modulus 20.0 GPa
2900 ksi
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) >= 290 °C
>= 554 °F
Electrical Properties Metric English Comments
Surface Resistance <= 1e+05
<= 1e+05
Insulation Resistance <= 100000 ohm
<= 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 310 °C
590 °F
mass temp
Nozzle Temperature 280 - 330 °C
536 - 626 °F
Zone 1 285 - 315 °C
545 - 599 °F
Zone 2 305 - 315 °C
581 - 599 °F
Zone 3 305 - 315 °C
581 - 599 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)
Users viewing this material also viewed the following: