Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resistance, non flammable.Antistatic.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0080 cm/cm
0.0020 - 0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Stress 160 MPa
23200 psi
Elongation at Yield 3.5 %
3.5 %
4.3 %
4.3 %
flexural
Modulus of Elasticity 11.0 GPa
1600 ksi
Flexural Strength 235 MPa
34100 psi
Flexural Modulus 9.00 GPa
1310 ksi
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
280 °C
536 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+10 ohm
<= 1.00e+10 ohm
Insulation Resistance <= 1.00e+10 ohm
<= 1.00e+10 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)