Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 11.0 - 23.5 GPa @Temperature 60.0 - 150 °C |
1600 - 3410 ksi @Temperature 140 - 302 °F |
Average value: 17.6 GPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/BK Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 527 |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 178 |
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |