Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Poco Graphite ACF-10Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Modulus of Elasticity | 11.0 - 13.0 GPa | 1600 - 1890 ksi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Modulus of Elasticity | 11.0 - 23.5 GPa @Temperature 60.0 - 150 °C |
1600 - 3410 ksi @Temperature 140 - 302 °F |
Average value: 17.6 GPa Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 11.0 - 26.2 GPa | 1600 - 3800 ksi | Average value: 17.2 GPa Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | 25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Modulus of Elasticity | 11.0 - 13.8 GPa | 1600 - 2000 ksi | Average value: 12.0 GPa Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 178 |
Addiplast Addinyl B2 ZV40 Nylon 6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |