Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 390 - 425 °C | 734 - 797 °F | Average value: 399 °C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 - 425 °C | 734 - 797 °F | |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/14 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7914 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Processing Temperature | 390 - 425 °C | 734 - 797 °F | |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |