Overview of materials for High Density Polyethylene (HDPE), Impact Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Impact Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.945 - 0.962 g/cc
0.0341 - 0.0348 lb/in³
Average value: 0.951 g/cc Grade Count:15
Viscosity 39000 - 480000 cP

@Temperature 190 - 190 °C
39000 - 480000 cP

@Temperature 374 - 374 °F
Average value: 164000 cP Grade Count:7
39000 - 480000 cP

@Shear Rate 300 - 5000 1/s
39000 - 480000 cP

@Shear Rate 300 - 5000 1/s
Average value: 164000 cP Grade Count:7
Environmental Stress Crack Resistance 1.00 - 500 hour
1.00 - 500 hour
Average value: 128 hour Grade Count:4
Melt Flow 0.300 - 42.0 g/10 min
0.300 - 42.0 g/10 min
Average value: 15.1 g/10 min Grade Count:15
Mechanical Properties Metric English Comments
Hardness, Shore D 59.0 - 64.0
59.0 - 64.0
Average value: 60.7 Grade Count:3
Tensile Strength, Ultimate 10.0 - 19.0 MPa
1450 - 2760 psi
Average value: 13.7 MPa Grade Count:8
Tensile Strength, Yield 17.2 - 25.0 MPa
2490 - 3630 psi
Average value: 21.5 MPa Grade Count:15
Elongation at Break 50.0 - 1000 %
50.0 - 1000 %
Average value: 415 % Grade Count:15
Modulus of Elasticity 0.510 - 1.10 GPa
74.0 - 160 ksi
Average value: 0.702 GPa Grade Count:10
Flexural Modulus 0.772 - 1.17 GPa
112 - 170 ksi
Average value: 0.903 GPa Grade Count:12
Izod Impact, Notched 0.534 - 3.74 J/cm
1.00 - 7.00 ft-lb/in
Average value: 1.60 J/cm Grade Count:3
Izod Impact, Notched (ISO) 27.0 - 176 kJ/m²
12.8 - 83.7 ft-lb/in²
Average value: 75.7 kJ/m² Grade Count:8
Falling Dart Impact 32.5397 - 176.257 J

@Temperature -40.0 - -40.0 °C
24.0000 - 130.000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 104 J Grade Count:2
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 73.0 °C
158 - 163 °F
Average value: 72.0 °C Grade Count:3
Vicat Softening Point 75.0 - 129 °C
167 - 264 °F
Average value: 114 °C Grade Count:11
Brittleness Temperature -118 - -75.0 °C
-180 - -103 °F
Average value: -94.3 °C Grade Count:4