Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | 5 mm/min |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | 5 mm/min |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Tensile Strength, Ultimate | 42.0 - 120 MPa | 6090 - 17400 psi | Average value: 83.0 MPa Grade Count:30 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Global N-3260 High Density Polyethylene, Yarn/Monofilament Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet
(discontinued **) Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® T Acrylic/PVC Thermoplastic Sheet Impact resistant fire rated sheetApplications: External housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for equipment such as v.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
KYDEX® V Acrylic/PC Thermoplastic Sheet Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Hannam Chemical Hanalac 775 ABS, Extrusion Grade Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Hannam Chemical Hanalac HFA-700 ABS |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Plenco 05118-T5 Phenolic, Granular, Injection Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Toyobo E2090A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polycaprolactone type, featuring a good balance of mechanical strength and chemical resistance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | DIN 53504 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 37 |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | DIN 53504 |
Lubrizol ESTANE® 58197 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 527-1 |
Chengdu Polyster H8570 Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 527-1 |
Chengdu Polyster H8570Y Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Low frictional coefficient and good abrasion resistance. Applications requiring high strength, high toughness .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D1708 |
DSM Biomedical BioSpan® F SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ISO 527 |
DSM Fibre Intermediates Nyrim® 2000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Tensile Strength, Ultimate | 42.0 - 80.0 MPa | 6090 - 11600 psi | Average value: 71.4 MPa Grade Count:12 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet
(discontinued **) General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy .. |
|||
Tensile Strength, Ultimate | 42.0 MPa | 6090 psi | ASTM D638 |
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, .. |