Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® APTIV® 2102-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled  (discontinued **

Category Polymer , Film , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® APTIV® 2102-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled  (discontinued **.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APTIV PEEK 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK 2100 has a unique combination of properties providing high temperature performance, light weight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen free and ease of processing makes APTIV films a technology enabler for our customers and end users. APTIV PEEK 2100 series provides a higher modulus over the APTIV 2000 series amorphous films. This grade is tailored towards thermoforming of thin wall parts with higher modulus, such as speaker diaphragms.Applications:Electrical InsulationAcoustic speaker diaphragmsThermoforming of thin wall partsAll information provided by Victrex.Properties measured on 50 micron film
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc

@Temperature 23.0 °C
1.42 g/cc

@Temperature 73.4 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break >= 200 %

@Temperature 23.0 °C
>= 200 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 527
Thermal Properties Metric English Comments
Shrinkage 2.0 - 4.0 %

@Temperature 200 °C
2.0 - 4.0 %

@Temperature 392 °F
TM-VX-84
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
100V; ASTM D257