Momentive Performance Materials RTV106 Red Adhesive Sealant, High Strength, High Temperature Paste

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV106 Red Adhesive Sealant, High Strength, High Temperature Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part alkoxy cure. Typical uses: High-heat applications; encapsulate and seal heating elements.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 2.55 MPa
370 psi
Elongation at Break 400 %
400 %
Adhesive Bond Strength 1.38 MPa
200 psi
Typical lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Continuous useful temperature.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 19.5 kV/mm
495 kV/in
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F