Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.206 GPa | 320.0 ksi | |
Abatron AboCast 8-19/Abocure 8-19 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c.. |
|||
Modulus of Elasticity | 2.206 - 2.344 GPa | 320.0 - 340.0 ksi | |
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
(discontinued **) Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical.. |
|||
Modulus of Elasticity | 2.206 GPa | 320.0 ksi | |
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet
(discontinued **) General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy .. |