Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact strength.Applications: pipe extrusion PE80 class, pressure pipe, drinking water and gas pipes, sewer pipes and their fittings, discharge pipes, for injection molded and other fittings, sheets.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ISO 1183
Melt Flow 0.45 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.45 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527-1
Elongation at Yield 8.0 %
8.0 %
ISO 527-1
Tensile Modulus 0.850 GPa
123 ksi
ISO 527-1
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 67.0 °C
153 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 136 °C
277 °F
190 - 220 °C
374 - 428 °F
Descriptive Properties Value Comments
Hydrostatic Strength, hr 1000
80°C; ISO 1167/DIN8075
MRS Classification, MPa 8
ISO/TR9080