3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abrasion and erosion resistanceProduct Features:Designed for application by trowel or spatulaDesigned for use to repair cracked pump housings, worn impellers, propellers, guide vanes, valves, and tube sheetsExcellent adhesion to correctly prepared metal surfaces Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness <= 305 microns
<= 12.0 mil
Mechanical Properties Metric English Comments
Flexural Strength 68.9 MPa
10000 psi
Compressive Strength 103 MPa
15000 psi
Shear Strength 17.2 MPa
2500 psi
Tensile Shear Adhesion
Abrasion 0.060
0.060
[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
Thermal Properties Metric English Comments
Heat Distortion Temperature 90.0 °C
194 °F
post cured 24 hrs at 100°C
Processing Properties Metric English Comments
Cure Time 7200 min
120 hour
Full Cure
Descriptive Properties Value Comments
Appearance Gray
Users viewing this material also viewed the following: